Material : X6CrNiNb18-10 ( 1.4550 )
Material Steel Number : 1.4550
Size : 2inch, 4inch , 8inch
Standard : ANSI B16.5
| Grade : | X6CrNiNb18-10 | ||||||||||||||
| Number: | 1.4550 | ||||||||||||||
| Classification: | Austenitic stainless steel - special grade | ||||||||||||||
| Density: | 7.9 g/cm ³ | ||||||||||||||
| Standard: | 
  | 
 
 
| Nb = 10 * C to 1.0 Elements not listed in this table shall not be intentionally added to the steel without the agreement of the purchaser except for finishing the cast.  | 
| C | Si | Mn | Ni | P | S | Cr | Nb | 
| max 0.08 | max 1 | max 2 | 9 - 12 | max 0.045 | max 0.015 | 17 - 19 | max 1 | 
| Rm - Tensile strength (MPa) (+A) | 500-740 | 
| Rm - Tensile strength (MPa) (+AT) | 510-740 | 
| Rp0.2 0.2% proof strength (MPa) (+AT) | 205 | 
| Rp0.2 0.2% proof strength (MPa) (+A) | 200-240 | 
| KV - Impact energy (J) transverse, (+A) | +20° 60  | -196° 40  | 
| KV - Impact energy (J) longitud., (+A) | +20° 100  | 
| A - Min. elongation at fracture (%) (+A) | 30-40 | 
| A - Min. elongation at fracture (%) longitud., (+AT) | 35 | 
| Brinell hardness (HB): (+A) | 230 | 
| Brinell hardness (HB): (+AT) | 210 | 
| Resistance to intergranular corrosion: in the delivery condition - yes; in the sensitized condition - yes Steel shal not be applied at a metal temperature lower than -196 ° C  | 
| EU EN  | USA -  | France AFNOR  | England BS  | Sweden SS  | Russia GOST  | |||||
| X6CrNiNb18-10 | 
  | 
  | 
  | 
  | 
  | 
| 
                                             | 
                